欢迎来到黄山市德邦粉体材料有限公司企业官网!

产品展示

TP20 Wrinkle Agent

2021-04-20     浏览次数:1152    

Description 

Winkle agent TP20 is also called as watermark agent. It is a kind of metal organic complexes which has a strong effect of curing acceleration, making the gel time very short and the coating has no time for leveling, thus can produce the well distributed wrinkle pattern like ground glass.

After the formula is adjusted, it is can produce sand texture, wrinkles and turtle shell textures.

 

Technical Parameters

Item

Test Methods

Specification

Appearance

Visualization

Yellowish powder

Melting Range (℃)

GB/T617-2006

190-196

Purity%

GB/T1725-2007

≥98.5

Curing Condition

180℃/20-25min;190℃/ 15min;200℃/10-12min.

 

Application

Used for producing fine wrinkle surface or other art powder such as sand texture and turtle shell texture .

 

Use method % characteristics

The dosage over 5wt% of the resin mixed with other materials and extruded .in the process of producing wrinkle coatings, the surface form is related to the dosage of TP20 and fillers. The more fillers used, the smaller wrinkle obtained.

 

Suggested Formulation

Raw material

Bottom powder

Formula 1

Formula 2

Formula

3 hybrid 7:3

remarks

Epoxy Resin E-12

60wt%

60

60

560-580


Polyester TP4060

3wt%

0

5

N/V

Use little 6:4 and 7:3 polyester to make texture big

Dicyandiamide

2.4wt%

3

3

22-24

Dosage :4-5% of epoxy

Wrinkle Agent TP20

3.6wt%

3

3

19-23

Can reduce to 2

Flowing Agent TP88

0.2wt%

0.2%

0.2%

2

Small dosage filler

gets big texture, Vice versa

Pigment and filler

30-50%

30-50%

30-50%

300-

500%

Eliminate pitting and bright spots

 

Extruding temperature: 90-100 °C, sieve through 140 mesh sieve

Due to the strong effect curing  acceleration of TP20, please extruding with low temperature

 

Take above formulation as base powder, than dry blending 0.1−0.2% TP80( turtle shell texture agent )can obtain turtle shell texture or snow pattern.

 

Spray thick thickness for big texture, otherwise, the coating will be shining; or spray thin thickness for small texture. Curing condition: 200°C/15min.

 

Used in hybrid or pure polyester system can get the effect of wrinkle and sand texture.

 

TP20  can also use as dry blending. Dry blending TP20 will consume smaller dosage compare with extruding, and the texture more coarse.

 

Try to not breathe the product dust for a long time, or else will arise symptoms feel like common cold. After disengagement of dust exposure, the symptoms will disappear in one week.

 

Package & Storage & Handling

1.Available in polyethylene-lined, multi-ply paper bags, N.W. 25KGS/Bag.

1. Storage in cool and dry place, avoid contact with skin and eyes; wear dust mask when operating; wash with water after operation.

2. Validity will be 1 years under normal temperature.

 


 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 

 


返回上一步
打印此页
QQ:1037432980
Skype:msjane881
微信公众号